I. Product introduction
4Cu + O2→2Cu2O
2Cu2O + O2→4CuO
AS-CU40 is extruded molding by adding binder to metal oxide. Oxygen removal is achieved by the reduction of high-valence metal oxides to low-valence metal oxides, which is achieved by the oxidation of the catalyst into copper oxide.
4Cu + O2→2Cu2O
2Cu2O + O2→4CuO
II. Technical introduction
AS-CU40 catalyst is applicable to oxygen removal in propylene, ethylene and inert gas. It is featured in good low temperature activity, high conversion rate, strong stability, high selectivity and long service life.
III. Typical parameter
1. Basic composition of the catalyst:
The catalyst is mainly composed of oxides of copper, zinc and aluminum, and contains a small amount of graphite and water.
Copper oxide: 38~43%
Zinc oxide 38~43%
Aluminum oxide: 6~9%
2. The main physicochemical properties of the catalysts:
Appearance: Black brown terete
Outline dimension: Φ5×5±1mm
Bulk density: 1150-1450 Kg/M3
Specific surface area: 60~110 m2/g
Radial crushing strength: Φ5: ≥120N/cm